Steel coil grades explained: DX51D, DD11, DC01

Steel coil grade names are built under EN 10027-1: the first letter D marks a flat product for cold forming, and the numbers rise with formability. DD11 to DD14 are hot rolled (EN 10111), DC01 to DC06 are cold rolled (EN 10130), and DX51D to DX57D are coated (EN 10346), where the suffix +Z or +AZ names the coating. Choose the grade by how hard the part is formed, and write the standard, grade and coating together in the enquiry.

Last updated

Key facts

  • Grade names follow EN 10027-1. For flat products the letter D marks steel for cold forming, and the numbers that follow rise with formability.
  • Hot rolled DD11 to DD14 are covered by EN 10111, and the standard ranks them by increasing formability from DD11 to DD14.
  • Cold rolled DC01 to DC06 are covered by EN 10130, and the numbers again rise with suitability for forming.
  • Coated DX51D to DX57D are covered by EN 10346. DX51D is bending and profiling quality and DX57D is super deep drawing quality, and the suffix +Z or +AZ names the coating.
  • Structural grades such as S220GD+Z to S550GD+Z are named by strength: the number is the minimum yield strength in MPa.

How is a steel coil grade name built?

Grade names are not trade names. They come from EN 10027-1, the European system for steel names, and each product standard applies it to its own grades. The standard lists letters for the application: S for structural steel, P for pressure purposes, H for high strength flat products and D for flat products for cold forming. After D, the grade carries a further letter and two numbers. The standard text previewed for this guide does not reproduce the full table, so the next paragraph reads the letters from the product standards instead.

In the three standards of the steel coil standards guide, the pattern is visible. The hot rolled grades of EN 10111 are DD11 to DD14, and the cold rolled grades of EN 10130 are DC01 to DC06. The coated grades of EN 10346 are DX51D to DX57D, where EN 10346 defines its low carbon steels by rolling type, hot or cold rolled, and a steel name from DX51D to DX57D, with higher grades corresponding to better formability. The letter after D therefore tells the rolling route in the first two cases (D for hot rolled, C for cold rolled), and X leaves the substrate open. Treat that reading of X as a guide and check it in the current EN 10027-1.

Each steel name also has a steel number under EN 10027-2. DX53D is 1.0355 in the EN 10346 text, for example, and the two forms can be used in an order. A name written with the +Z suffix, such as DX53D+Z, is the name plus the coating symbol.

What do DD11 to DD14 mean on hot rolled coil?

EN 10111 specifies continuously hot rolled low carbon steel sheet and strip supplied in coils for cold forming, in thicknesses from 1.0 mm to 11 mm (0.039 to 0.433 in) [0.039 to 0.43 in]. Its four grades, DD11, DD12, DD13 and DD14, are defined by chemical composition and by mechanical and forming characteristics, and the standard says they correspond to increasing formability in that order. For DD11 the method of deoxidation is left to the manufacturer, while DD12, DD13 and DD14 are fully killed.

The pickled and oiled hot rolled coil page lists DD11 to DD14 beside the structural grades S235JR, S275JR and S355JR and the high yield grades S315MC to S700MC. These belong to other standards (EN 10025-2 and EN 10149-2) and are named by yield strength, not by forming class. The range sourced here starts at 0.80 mm (0.031 in) [0.031 in], below the 1.0 mm (0.039 in) lower limit of EN 10111, so the mill confirms the standard and the thickness together.

EN 10111 also notes that descaled coil is usually delivered oiled, and that the oil protects against corrosion for a limited period under normal storage, which is another reason to state the date you need the coil.

What do DC01 to DC06 mean on cold rolled coil?

EN 10130 covers cold rolled uncoated low carbon steel flat products for cold forming, in widths from 600 mm (23.62 in) [23.6 in], from a minimum thickness of 0.35 mm (0.014 in) [0.014 in] up to 3 mm (0.12 in) [0.118 in] unless otherwise agreed. The grades start at DC01 and rise to DC03, DC04, DC05, DC06 and DC07. The cold rolled coil page lists DC01, DC03, DC04, DC05 and DC06.

Two details matter when choosing. First, deoxidation: DC01 is left to the manufacturer, while DC03 and above must be aluminium fully killed. Second, time. The standard sets no time limit on the mechanical properties of DC01 and holds DC03 to DC07 to their values for 6 months from availability at the mill, and it notes that long storage of DC01 can reduce formability. Grades DC06 and DC07 do not show stretcher strain marks. For how the strip is annealed and skin passed to reach these properties, see hot rolled vs cold rolled coil.

What do DX51D to DX57D mean on coated coil?

EN 10346 ranks the low carbon steels for cold forming by increasing suitability for forming, which makes the decision table below simple to read.

EN 10346 low carbon steels for cold forming, ranked by suitability for forming
GradeSteel numberForming quality in EN 10346
DX51D1.0226Bending and profiling
DX52D1.0350Drawing
DX53D1.0355Deep drawing
DX54D1.0306Special deep drawing
DX56D1.0322Extra deep drawing
DX57D1.0853Super deep drawing

DX55D exists in the standard text read for this guide, but only with an aluminium-silicon coating, so it is not a galvanized grade. In the same text DX57D is listed with the zinc coating but not with +AZ. Check the current edition before ordering a combination.

The suffix names the coating: +Z is zinc, +ZF zinc-iron, +ZA zinc-aluminium, +ZM zinc-magnesium, +AZ aluminium-zinc and +AS aluminium-silicon. The galvanized coil page lists DX51D+Z to DX57D+Z and the structural S220GD+Z to S550GD+Z, and the prepainted steel coil page lists DX51D+Z to DX54D+Z and S220GD+Z to S350GD+Z as its base steels.

In the structural grades, the number is not a forming class. EN 10346 ranks them by increasing minimum proof strength, and EN 10027-1 names them by minimum yield strength in MPa, so S350GD+Z is a 350 MPa grade. The standard also covers high proof strength grades for cold forming, which the page does not list, so confirm them separately. EN 10346 states that ageing can reduce formability and cause coil breaks or fluting, and that the risk grows with storage time, so plan the order close to the time of use.

How do you choose a grade?

Start from the forming operation and the thickness, not from the grade name.

Grade families compared by duty
If the part needsLook atStandard
Bending, profiling, roll forming with zinc protectionDX51D+ZEN 10346
Pressing or drawing with zinc protectionDX52D+Z to DX57D+ZEN 10346
Strength first, with zinc protectionS220GD+Z to S550GD+ZEN 10346
Drawing on uncoated cold rolled stripDC01 to DC06EN 10130
Thicker hot rolled strip for formingDD11 to DD14EN 10111
Structural or high yield hot rolledS235JR to S355JR; S315MC to S700MCEN 10025-2; EN 10149-2

Three rules keep the choice practical. Pick the lowest grade that forms the part without cracking, because the standards state that formability rises with the number. Match the grade to the coating, since the coating decides which suffix exists. And state thickness with the grade, because the standards start at different thicknesses.

What should the order say?

Name the standard, the grade and, for coated coil, the coating symbol and mass in that order, for example EN 10346 DX51D+Z275. The EN 10346 text read for this guide lists the steel name or number with the coating symbol, the nominal coating mass, the coating finish, the surface quality and the surface treatment among the details a purchaser states. The details of coating mass are in galvanized vs Aluzinc coil, and the choice between narrow and wide coil in slit coil vs full-width coil.

Reinwent is a trading and sourcing company that sources coil from manufacturers in Tรผrkiye. Send the grade, thickness, width and end use with your quote request, and the whole range is on the steel coil page.

Related coil guides: coil thickness and width; galvanized coil finish and spangle; cold rolled coil annealing.

Questions buyers ask

What does DX51D mean?

DX51D is a low carbon steel for cold forming in EN 10346, the standard for continuously hot-dip coated flat products. The D marks a flat product for cold forming, and the standard classes DX51D as bending and profiling quality. The coating is added as a suffix, so DX51D+Z is zinc coated and DX51D+AZ is aluminium-zinc coated.

Which is the better forming grade, DX51D or DX54D?

DX54D. EN 10346 ranks the DX grades by increasing suitability for cold forming: DX51D is bending and profiling quality, DX52D drawing, DX53D deep drawing, DX54D special deep drawing, DX56D extra deep drawing and DX57D super deep drawing. Higher grades suit harder forming, so choose the lowest grade that forms your part without cracking.

What is the difference between DC01 and DD11?

They are different products under different standards. DC01 is a cold rolled grade in EN 10130, and DD11 is a hot rolled grade in EN 10111. The thickness ranges differ too: EN 10130 starts at 0.35 mm (0.014 in) [0.014 in] and EN 10111 starts at 1.0 mm (0.039 in) [0.039 in], so the thickness you need often decides the family.

What does S220GD+Z or S350GD+Z mean?

S marks a structural steel, and in EN 10027-1 the number is the minimum yield strength in MPa, so S350 is 350 MPa. In EN 10346 the structural grades are ranked by increasing minimum proof strength, and +Z shows the zinc coating. Use these grades when strength matters more than deep forming.

Do the mechanical properties of a grade last forever?

No. Steel ages, and forming grades lose some formability in storage. EN 10130 sets no time limit on the properties of DC01 and holds DC03 to DC07 to their values for 6 months from availability at the mill, and EN 10346 advises processing coated coil soon after receipt. Order for the time you will actually need to store the coil.

Can an EN grade be matched to an ASTM grade?

Not one-to-one. ASTM A653 names its forming levels in words, such as commercial, forming, deep drawing and extra deep drawing steel, and also has structural and high strength low alloy designations. EN 10346 names them DX51D to DX57D and S220GD to S550GD. The two systems differ in tests and limits, so state the ASTM designation you need and let the mill answer whether it can supply it or propose the nearest EN grade for you to approve.

What should I write about the grade in a coil enquiry?

Give the standard and the grade, with the coating suffix and coating mass for coated coil (for example EN 10346 DX51D+Z275), the thickness and width in millimetres, whether the coil is full-width or slit, and the end use. For cold rolled coil add the surface quality and finish, and say if you need the grade for deep drawing. Reinwent sends the quotation within 12 hours at the latest.

Sources

Request a quote

Tell us the specification you need and we will check it with manufacturers in Tรผrkiye. We reply with a quotation within 12 hours.

Request a quote