Does galvanized wire rust? Coating life explained

Galvanized wire does rust eventually, but only after the zinc coating has been used up. Hot-dip galvanizing corrodes at about 1/30 of the rate of bare steel in the same setting, and the coating thickness and the environment decide how long the zinc lasts.

Last updated

Key facts

  • Galvanized wire can rust, but only after its zinc coating has been used up.
  • Hot-dip galvanizing corrodes at about 1/30 of the rate of bare steel in the same environment, according to the American Galvanizers Association.
  • Coating thickness is the main factor in how long the zinc lasts, and the environment changes the result.
  • Zinc also protects steel at small cuts and scratches, so a cut end does not start to rust at once.
  • Hot-dip coatings are thicker than electro-galvanized ones, and black annealed wire has no zinc at all.

The short answer

Yes, galvanized wire does rust, but it takes much longer than bare steel. The zinc on the surface corrodes first and slowly, and the steel only starts to rust when the zinc in that spot has been consumed. How long that takes depends on how much zinc the wire carries and where the wire is used. This guide explains the mechanism and what to put on an order so the coating fits the job.

How zinc protects steel

Zinc protects steel in two ways. The first is as a barrier: the coating sits between the steel and the air, and, in the words of the Wikipedia article on galvanization, it โ€œprevents corrosive substances from reaching the underlying ironโ€ while it is intact.

The second is sacrificial protection. Zinc is more reactive than iron, so it oxidizes first and acts as a sacrificial anode. That is why a small scratch does not let the steel rust straight away.

The American Galvanizers Association adds that hot-dip galvanizing generally corrodes at a rate of 1/30 of bare steel in the same environment. It also notes that zincโ€™s corrosion products are adherent and fairly insoluble in most environments, so the corrosion rate often slows as time progresses.

What decides how long the coating lasts

Two things matter most.

Coating thickness. According to the American Galvanizers Association, the corrosion resistance of a zinc coating is determined primarily by its thickness. On wire, thickness is set through the coating class, which fixes the zinc mass per square metre for each diameter. Our guide to zinc coating classes shows EN 10244-2 and ASTM A641 side by side.

The environment. The same association points out that each environment affects hot-dip galvanizing differently, because each has its own set of corrosion variables. Damp, salty or polluted air uses zinc faster than dry, clean air.

Because of this, no single figure can say how long galvanized wire lasts. We do not state a service life: it depends on the class you order and the place the wire is used.

Cut ends and scratches

When wire is cut or scratched, the steel is exposed. Wikipedia explains that zinc can continue to protect the steel through galvanic corrosion, and that this is often effective within an annulus of about 5 mm (0.20 in). Beyond that distance the protective effect fades. For binding or tying wire that is cut on site, the cut ends are therefore protected by the zinc beside them.

Hot-dip, electro-galvanized and black annealed compared

Finish Zinc on the wire What it means for rust
Hot-dip galvanized A thick, robust layer of zinc-iron alloys The longest protection of the three at the same diameter
Electro-galvanized A thinner layer of zinc Protects, but with less zinc to use up
Black annealed No zinc coating Rusts as bare steel does

For the process behind the first two rows, see hot-dip vs electro-galvanized wire and the steps of hot-dip galvanizing for wire. If you are choosing between a galvanized and an uncoated wire for tying, read black annealed vs galvanized tie wire.

Choosing a coating class when you order

A practical order names the standard and the class, or gives the coating mass you need in g/mยฒ. ASTM A641 covers zinc-coated carbon steel wire in coils for general use, and EN 10244-2 covers zinc and zinc alloy coatings on steel wire. The two define their classes separately, so name one standard per order. Say where the wire will be used, because that is what the class should match.

Reinwent is a trading and sourcing company. For hot-dip galvanized wire, the product page lists the diameter and coating range, and the page on galvanized wire from Tรผrkiye explains how an order runs from specification to shipping. To compare classes for your use, send the enquiry through the quote form; the quotation comes within 12 hours.

Questions buyers ask

Does galvanized wire rust?

Yes, in the end. The zinc coating is used up slowly, and the steel under it can rust once the zinc is gone. While zinc remains, it protects the steel.

Does a thicker zinc coating last longer?

Yes. The American Galvanizers Association states that the corrosion resistance of a zinc coating is determined primarily by its thickness, and that the severity of the environment changes the result. A heavier coating class carries more zinc.

Does galvanized wire rust faster near the sea or in industrial air?

The environment matters. The American Galvanizers Association notes that each environment affects hot-dip galvanizing differently. If the wire will work near the coast or in industrial air, tell the supplier and ask for a heavier coating class.

Does a cut end of galvanized wire rust?

A cut exposes bare steel, but zinc is more reactive than iron and keeps protecting nearby steel by galvanic action. Wikipedia describes this as often effective within about 5 mm (0.20 in) of the zinc, so a cut end is not a coating failure.

Does black annealed wire rust?

Yes, and faster, because black annealed wire carries no zinc coating. Our comparison of black annealed and galvanized tie wire shows when each is used.

How do I order wire that resists rust for longer?

Name the standard and the coating class, or the coating mass in g/mยฒ, on the enquiry. Heavier classes carry more zinc, and the final class and mass are confirmed in the quotation.